首页> 外国专利> AMORPHOUS BLEND COMPRISING AN AMORPHOUS SEMIAROMATIC POLYAMIDE AND A SEMICRYSTALLINE POLYAMIDE OF NYLON TYPE

AMORPHOUS BLEND COMPRISING AN AMORPHOUS SEMIAROMATIC POLYAMIDE AND A SEMICRYSTALLINE POLYAMIDE OF NYLON TYPE

机译:包含非晶型亚氨基聚丙烯酸酯和尼龙型半结晶聚丙烯酰胺的非晶态共混物

摘要

Single-phase and amorphous polymeric mixtures capable of being employed especially for producing shaped articles using moulding operations. According to the invention the said mixtures comprise: (i) an amorphous semiaromatic polyamide obtained from 2-methyl-1,5-pentamethylenediamine taken by itself or mixed with 2-ethyl-1,4-tetramethylenediamine and isophthalic acid taken by itself or mixed with terephthalic acid, and (ii) a semicrystalline polyamide of the nylon type chosen from the group made up of nylon 66, nylon 6, mixtures of these polymers and the copolymers obtained from monomers resulting in these nylons, the quantity of the semicrystalline polyamide of the nylon type (ii) representing not more than 40% of the weight of the combined semiaromatic polyamide (i) + semicrystalline polyamide (ii). The resilience properties of the semiaromatic polyamide at temperatures ranging from room temperature to -25 DEG C can be improved with such mixtures.
机译:单相和无定形聚合物混合物能够特别用于通过模塑操作生产成型制品。根据本发明,所述混合物包括:(i)由2-甲基-1,5-五亚甲基二胺本身或与2-乙基-1,4-四亚甲基二胺和间苯二甲酸自身或混合获得的无定形半芳族聚酰胺。 (ii)选自尼龙66,尼龙6的尼龙类型的半结晶聚酰胺,这些聚合物的混合物以及由得到这些尼龙的单体得到的共聚物,该半结晶聚酰胺的量为尼龙类型(ii)占组合的半芳族聚酰胺(i)+半结晶聚酰胺(ii)重量的不超过40%。用这种混合物可以改善半芳族聚酰胺在室温至-25℃的温度下的回弹性。

著录项

  • 公开/公告号AU5876890A

    专利类型

  • 公开/公告日1991-01-17

    原文格式PDF

  • 申请/专利权人 RHONE-POULENC CHIMIE;

    申请/专利号AU19900058768

  • 发明设计人 DANIEL ROBERJOT;JEAN-PIERRE PREVOST;

    申请日1990-07-09

  • 分类号C08L77/00;C08J5/00;

  • 国家 AU

  • 入库时间 2022-08-22 05:55:17