It is described as polyblend of polyurethane and nitrile rubber, a thermoplastic polyurethane elastomer without containing a plasticizer, has a hardness of 55 to 70 Shore A. The polyurethane component contains a polyisocyanate content of at least 50 wt .-%; the acrylonitrile content in the rubber component is 34 mol% and the ratio of polyurethane to the; Nitrile component amounts to 30:70 to 40:60 vol .-%. Further, a manufacturing method is provided, wherein said polyurethane having a hardness of 80 to 90 Shore A and a minimum polyisocyanate content of 50 wt .-% of a nitrile rubber having a viscosity ML 1 + 4,100 ° C = 50 and having an acrylonitrile content is processed rubber of 30:70 to 40:60 by mixing and kneading at 180 to 215 ° C to a polyblend: from 34 mol% in volume percentage ratio of polyurethane.
机译:它被描述为聚氨酯和丁腈橡胶的一种共混物,一种不含增塑剂的热塑性聚氨酯弹性体,硬度为55至70肖氏A。聚氨酯组分的多异氰酸酯含量至少为50 wt .-%。橡胶组分中的丙烯腈含量为34mol%,聚氨酯与聚氨酯的比例为腈成分为30:70至40:60vol .-%。此外,提供了一种制造方法,其中,所述聚氨酯的粘度为 ML 1 + 4,100°,其硬度为80至90肖氏A,最小多异氰酸酯含量为50 wt .-%的丁腈橡胶。 C = 50且具有丙烯腈含量的橡胶通过在180至215℃下混合并捏合成多掺混物而以30:70至40:60的比例加工成聚氨酯:以体积百分比计为34摩尔%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号