Viscoelastic flexible PU foam material (I) are produced by reaction of (a) opt. modified polyisocyanates with (b) mixts. of polyether-polyols (b1) and polyester-polyols (b2) and opt. (c) low- mol.wt. chain-extenders in the presence of (d) catalysts, (e) blowing agents and opt. (f) other additives and auxiliary substances; the novelty is that (b2) are dipropylene glycol-adipic acid polyesters with OH no. 20-150. Mixts. (b) are claimed, comprising 15-50 pts.wt. polyether-polyols, polyoxypropylenepolyoxyethylene-polyols, polymer-modified polyoxyalkylene-polyols or mixts. of at least 2 of these types, and 50-85 pts.wt. (b2) as in 1. above. USE/ADVANTAGE - (I) are useful for the prodn. of sound insulating foam liners, etc., esp. to reduce the noise level in motor vehicles and machines; other applications include carpet backing, furniture, building components, etc. The invention provides (I) with improved relaxation properties, resulting in better sound insulation; the starting materials are relatively inexpensive, and miscible in the required proportions.
机译:粘弹性软质PU泡沫材料(I)通过(a)opt的反应生产。 (b)混合物的改性多异氰酸酯。聚醚多元醇(b1)和聚酯多元醇(b2)的选择。 (c)低分子量(d)催化剂,(e)发泡剂和opt。 (f)其他添加剂和辅助物质; (b2)是OH号为0的二丙二醇-己二酸聚酯。 20-150。混音。 (b)要求保护,包括15-50pts.wt。聚醚-多元醇,聚氧丙烯-聚氧乙烯-多元醇,聚合物改性的聚氧化烯-多元醇或混合物。这些类型中的至少2种,以及50-85pts.wt。 (b2)如上述1.。使用/优势-(I)对产品有用。隔音泡沫衬里等,尤其是降低机动车辆和机器的噪音水平;其他应用包括地毯背衬,家具,建筑部件等。起始原料相对便宜,并且可以所需比例混溶。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号