Description of the preparation of a Ziegler type catalyst system through impregnation of a special alumina with 0.8-1.0% by weight of titanium derived from a dilute solution of titanium halide in n-hexane, the activator employed being triisobutylaluminum or triethylaluminum at an (Al)/(Ti) molar ratio of 2.5/1 to 80/1 in the catalyst. The catalyst system has high efficiency and yield, and leads to polyethylenes of excellent physical and mechanical properties which make it particularly suitable for use in engineering plastics.
机译:通过用特殊的氧化铝浸渍0.8-1.0%重量的钛(从卤化钛的正己烷稀溶液中衍生)来制备齐格勒型催化剂体系的说明,所用的活化剂为三异丁基铝或三乙基铝,(Al) /(Ti)在催化剂中的摩尔比为2.5 / 1至80/1。该催化剂体系具有高效率和产率,并导致具有优异的物理和机械性能的聚乙烯,这使其特别适用于工程塑料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号