A process for producing a Cu-Fe-Co-Ti alloy useful as conductor elements in the electronics and connector industries. The alloy is produced in the form of a bath having a Ti/Fe+Co ratio between 0.3 and 1 and a Co/Fe ratio between 0.10 and 0.90. The molten alloy bath is deoxidized with boron, cast, homogenized, cold drawn, and subjected to a precipitation heat treatment at a temperature lower, by at most 80° C. , than a temperature TM leading to the maximum electric conductivity.
机译:生产用于电子和连接器行业中的导体元素的Cu-Fe-Co-Ti合金的方法。所述合金以浴的形式生产,所述浴的Ti / Fe + Co比为0.3至1,并且Co / Fe比为0.10至0.90。用硼对熔融合金浴进行脱氧,铸造,均质化,冷拔,并在比导致最大导电率的温度TM低至多80℃的温度下进行沉淀热处理。

著录项

  • 公开/公告号US5026434A

    专利类型

  • 公开/公告日1991-06-25

    原文格式PDF

  • 申请/专利权人 TREFIMETAUX;

    申请/专利号US19900542919

  • 申请日1990-06-25

  • 分类号C22F1/08;C22C9/00;

  • 国家 US

  • 入库时间 2022-08-22 05:46:20

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号