FE-CR-NI-SI SHAPE MEMORY ALLOY EXCELLENT IN SHAPE MEMORY CHARACTERISTIC, CORROSION RESISTANCE, AND STRESS CORROSION CRACKING RESISTANCE

机译:FE-CR-NI-SI形状记忆合金在形状记忆特性,耐腐蚀性和应力腐蚀开裂性方面表现优异

摘要

PURPOSE:To obtain the alloy suitable for use in a nuclear power field, etc., by specifying the contents of Cr, Si, and Ni, respective total contents of austenite forming elements and ferrite forming elements, and the total content of Cr and Si, respectively. CONSTITUTION:This Fe-Cr-Ni-Si shape memory alloy has a composition which consists of, by weight, 16.0-21.0% Cr, 3.0-7.0% Si, 11.0-21.0% Ni, and the balance Fe and in which Ni=[0.67(Cr+1.2Si)-3] and (Cr+Si)=20 are satisfied. Moreover, 0.1-5.0% Mn, 0.1-1.0% Cu, 0.001-0.100% N, 0.1-3.0% Mo, and 0.1-3.0% W can be further incorporated into the above alloy.
机译:目的:通过指定Cr,Si和Ni的含量,奥氏体形成元素和铁素体形成元素的各自总含量以及Cr和Si的总含量,来获得适用于核动力领域等的合金, 分别。组成:这种Fe-Cr-Ni-Si形状记忆合金具有以下组成:按重量计包括16.0-21.0%Cr,3.0-7.0%Si,11.0-21.0%Ni和余量的Fe,其中Ni> = [0.67(Cr + 1.2Si)-3]且(Cr + Si)> = 20。另外,在上述合金中可以进一步含有0.1〜5.0%的Mn,0.1〜1.0%的Cu,0.001〜0.10%的N,0.1〜3.0%的Mo,0.1〜3.0%的W。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号