SUBMERGED ARC WELDING METHOD FOR CR-MO LOW ALLOY STEEL

机译:铬钼低合金钢的埋弧焊接方法

摘要

PURPOSE:To improve the weld strength by using a wire containing specific amounts of Cr and Mo and baked flux containing CaF2 and metallic carbonate and further, adding specific components to one side or both sides of the wire or the flux. CONSTITUTION:The wire containing 1.80-3.80% Cr and 0.80-1.30% Mo and not containing Ti and Nb substantially and the baked flux containing 10-20% CaF2 and the metallic carbonate equivalent to 2.5-10% CO2 and not containing Ti, a Ti oxide, Nb, and an Nb oxide substantially are used and further, C, Si, Mn, V (or V2O5) and B (or B2O3) are added to either one side or both sides of the wire or the flux so as to satisfy formulas and the welding is performed. By this method, the satisfactory weld strength can be obtained.
机译:目的:通过使用包含特定量的Cr和Mo的焊丝以及包含CaF2和金属碳酸盐的烘焙助焊剂,并进一步在焊丝或助焊剂的一侧或两侧添加特定成分,以提高焊接强度。组成:含有1.80-3.80%Cr和0.80-1.30%Mo且基本上不含Ti和Nb的焊丝,以及含10-20%CaF2和相当于2.5-10%CO2且不含Ti的金属碳酸盐的烘烤助焊剂,基本上使用Ti氧化物,Nb和Nb氧化物,然后将C,Si,Mn,V(或V2O5)和B(或B2O3)添加到焊丝或焊剂的一侧或两侧,以便满足公式并执行焊接。通过这种方法,可以获得令人满意的焊接强度。

著录项

  • 公开/公告号JPH042349B2

    专利类型

  • 公开/公告日1992-01-17

    原文格式PDF

  • 申请/专利权人

    申请/专利号JP19870070223

  • 发明设计人

    申请日1987-03-26

  • 分类号B23K9/18;B23K9/23;B23K35/30;B23K35/362;

  • 国家 JP

  • 入库时间 2022-08-22 05:41:33