首页> 外国专利> Process for preparing a body ceramico, body ceramico and cutting tool

Process for preparing a body ceramico, body ceramico and cutting tool

机译:制备陶瓷体的方法,陶瓷体和切削工具

摘要

A process for preparing a self-reinforced silicon nitride ceramic body of high fracture toughness comprising hot-pressing a powder mixture containing silicon nitride, a densification aid such as sodium oxide, a conversion aid such as lanthanum oxide and a compound, such as gallium oxide, which enhances growth of beta -silicon nitride whiskers-under conditions such that densification and the in situ formation of beta -silicon nitride whiskers having a high aspect ratio occur. A novel silicon nitride ceramic of high fracture toughness and high fracture strength is disclosed comprising a beta -silicon nitride crystalline phase wherein at least 20 volume percent of the phase is in the form of whiskers having an average aspect ratio of at least 2.5; a glassy second phase containing the densification aid, the conversion aid, the compound which enhances growth of beta -silicon nitride whiskers, and an amount of silica; and not greater than 10 weight percent of the total weight as other phases. The glassy phase may also include a minor amount, e.g., up to 5.0 weight percent, based upon total weight of the ceramic, of aluminum nitride or boron nitride. The glassy phase optionally includes an amount of a secondary reinforcing material such as silicon carbide whiskers.
机译:一种制备高断裂韧性的自增强氮化硅陶瓷体的方法,包括热压包含氮化硅,致密助剂如氧化钠,转化助剂如氧化镧和化合物如氧化镓的粉末混合物。在出现高纵横比的β-氮化硅晶须的致密化和原位形成的条件下,其增强了β-氮化硅晶须的生长。公开了一种具有高断裂韧性和高断裂强度的新型氮化硅陶瓷,其包含β-氮化硅结晶相,其中所述相的至少20体积%为晶须的形式,所述晶须的平均长径比为至少2.5;含有致密化助剂,转化助剂,增强β-氮化硅晶须生长的化合物和一定量二氧化硅的玻璃态第二相;不超过其他相总重的10%(重量)。基于陶瓷的总重量,玻璃相还可包含少量,例如至多5.0重量%的氮化铝或氮化硼。所述玻璃相任选地包含一定量的辅助增强材料,例如碳化硅晶须。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号