PURPOSE:To provide a shrinkable film for plastic bottle, composed of a composition produced by compounding a polyvinyl chloride resin with a specific plasticizer, having high thermal stability, shrinking stress and rigidity and suitable especially for the after-labeling of a PET bottle shoulder. CONSTITUTION:The objective shrinkable polyvinyl chloride film for plastic bottle has lateral thermal shrinkage of 10-20% by the hot-water immersion at 70 deg.C for 10sec and 55-60% at 85 deg.C for 10sec. It can be produced by compounding (A) 100 pts.wt. of a polyvinyl chloride resin having an average polymerization degree of 800-2,500 (preferably 1,000-1,800) with (B) 2-7 pts.wt. of plasticizers consisting of (B1) one or more kinds of esters selected from dialkyl phthalate, dialkyl adipate and trialkyl trimellitate (preferably 7-12C alkyl ester such as dioctyl phthalate) and (B2) dicyclohexyl phthalate at a weight ratio (B1:B2) of 1:2 to 2:1, forming the obtained resin composition in the form of a film and drawing the film.
机译:用途:提供一种用于塑料瓶的可收缩薄膜,其由通过将聚氯乙烯树脂与特定的增塑剂混合而制成的组合物组成,具有高的热稳定性,收缩应力和刚性,特别适合于PET瓶肩的后标签。组成:用于塑料瓶的目标可收缩聚氯乙烯薄膜通过在70℃下热水浸泡10秒和在85℃下10秒浸泡55-60%,具有10-20%的横向热收缩率。可以通过混合(A)100 pts.wt来生产。聚氯乙烯树脂的平均聚合度为800-2,500(最好为1,000-1,800),(B)为2-7pts.wt。增塑剂组成,其重量比为(B1:B2),由(B1)一种或多种选自邻苯二甲酸二烷基酯,己二酸二烷基酯和偏苯三酸三烷基酯(最好是7-12C烷基酯,例如邻苯二甲酸二辛酯)和(B2)邻苯二甲酸二环己酯的酯组成以1∶2至2∶1的比例,以膜形式形成所获得的树脂组合物并拉伸该膜。

著录项

  • 公开/公告号JPH04370132A

    专利类型

  • 公开/公告日1992-12-22

    原文格式PDF

  • 申请/专利权人 C I KASEI CO LTD;

    申请/专利号JP19910173287

  • 发明设计人 WADA NOBUAKI;

    申请日1991-06-19

  • 分类号B29C61/06;B65B53/04;C08J5/18;C08K5/10;C08L27/06;

  • 国家 JP

  • 入库时间 2022-08-22 05:14:43

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号