The present Invention relates to a method for inhibiting the Corrosion Cracking due to effort, mainly attributable to exposure to irradiation ConcentratedIn austenitic Alloys that contain high levels of nickel and ChromiumIt is characterized because the mass of the Alloy at a temperature within the range of 1121 degrees C at least until around 1315 degrees C for a period of at least 1 minutAbout 45 minutes or so, the period of Heat Treatment of the Alloy is approximately inversely proportional to the temperature treatment.
机译:本发明涉及一种抑制由于腐蚀而产生的腐蚀开裂的方法,该方法主要归因于暴露于辐照下。浓缩在含有高含量的镍和铬的奥氏体合金中。其特征在于,合金的质量在1121度范围内至少直到大约1315℃,持续至少1分钟的时间,大约45分钟左右,合金的热处理时间与温度处理成反比。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号