首页> 外国专利> Recovery of Iron from ferrous slag in the form of a Concentrate by Magnetic sorting

Recovery of Iron from ferrous slag in the form of a Concentrate by Magnetic sorting

机译:通过磁选从精矿中回收铁渣中的铁

摘要

The invention refers to the recovery of iron in the form of concentrate from iron furnace slag by magnetic classification. The method is to classify the slag with a volume of more than 300 mm to 500 mm extracted from the furnace and a volume of more than 300 mm to 500 mm into various stages of magnetic classification: 2. If the iron content is more than 50-60%, the iron content of the slag with the iron content less than 50-60% is more than 50-60%; for the slag with the iron content more than 50-60%, the compression force is applicable, so as to reduce its volume from the above value;This recovery method is to classify the slag whose volume is less than the above-mentioned value into slag with iron content more than 50-60% and slag with iron content less than 50-60%. 1. Slag with crushing volume less than the above value and iron content more than 50-60%; 1. The crushed products are screened with pre-determined mesh size to produce slag less than 40 mm and concentrate with high iron content of about 40 mm;Concentrate is collected for later use in iron and steel production.
机译:本发明涉及通过磁选从铁炉渣中回收精矿形式的铁。该方法是将从炉中取出的大于300 mm至500 mm的炉渣和大于300 mm至500 mm的炉渣分类到磁分级的各个阶段:2.如果铁含量大于50 -60%时,铁含量小于50-60%的炉渣中铁含量大于50-60%;铁含量大于50-60%的炉渣,可施加压缩力,以使其体积从上述值减小;该回收方法是将小于上述值的炉渣分类为铁含量大于50-60%的炉渣,铁含量小于50-60%的炉渣。 1.破碎量小于上述值且铁含量大于50-60%的炉渣; 1.将粉碎的产品以预定的筛目进行筛分,以产生小于40 mm的炉渣,并含铁约40 mm的高铁精矿;收集精矿用于钢铁生产。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号