WHOLLY AROMATIC POLYESTER FIBER-REINFORCED HIGH PERFORMANCE THERMOPLASTIC AND PROCESS FOR PREPARING SAME
WHOLLY AROMATIC POLYESTER FIBER-REINFORCED HIGH PERFORMANCE THERMOPLASTIC AND PROCESS FOR PREPARING SAME
展开▼
机译:全芳香族聚酯纤维增强的高性能热塑性塑料及其制备方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
Self-reinforced polymer composities of 60-5 percent by weight of an at least partially crystalline high performance thermoplastic polymer and 40-95 percent by weight of a melt processable wholly aromatic polyester which exhibit anisotropic properties in the melt phase. This wholly aromatic polyester is a liquid crystal polymer, or LCP. The high performance themoplastic polymer has a melting point of at least 200 DEG . Polyether etherketone is a preferred at least partially crystalline polymer. The wholly aromatic polyester is in the form of predominantly unidirectionally oriented continuous fibers primarily in the range of about 1 to 10 micrometers in diameter, distributed in a matrix of polyether etherketone. The polymer composites of this invnetion have high tensile strength, high modulus, satisfactory elongation, good impact strength, and good high temperature properties.
展开▼