High-mol. wt. thermoplastic polyurethane (TPU) elastomers (I) are prepd. by adding 0.05-5 wt.% organic di-isocyanate (II) to a conventional TPU elastomer (III) during thermoplastic processing, and conditioning the moulding material obtd. for at least 1 hr. at 50-150 deg.C. Specifically amt. of (II) is 0.2-3 wt.%. (III) is a polyester- or polyether-urethane derived from long-chain OH cpds. with mol.wt. 500-3000, short-chain aliphatic and/or aromatic diols with mol.wt. below 600, aromatic cyclic and/or aliphatic di-isocyanates and opt. stabilisers, additives etc. (II) is an aliphatic and/or aromatic ring-contg. di-isocyanate and/or a di-isocyanate-producing cpd. and/or a NCO-terminated prepolymer with mol.wt. below 5000; (II) is added to the polymer melt as a solid or liq., via the feed opening or feed zone or at another suitable point in the extruder or injection moulding machine, or (II) is premixed with (III) outside the processing machine, and the wetted granules are then processed as usual. After processing or final moulding, the material is conditioned for at least 1 (pref. 24) hrs. at 50-150 (pref. 100) deg.C. USE/ADVANTAGE - Addn. of (II) increases the mol.wt. of the TPU, giving TPU elastomers with improved hydrolytic stability and wear resistance (for prodn. of coatings, tubes, profiles, wearing parts etc.).
机译:高摩尔重量准备热塑性聚氨酯(TPU)弹性体(I)。通过在热塑性加工过程中向常规的TPU弹性体(III)中添加0.05-5重量%的有机二异氰酸酯(II),并调节成型材料obtd。持续至少1小时。在50-150摄氏度特别是amt。 (II)的含量为0.2-3重量%。 (III)是衍生自长链OH cpds的聚酯或聚醚-氨基甲酸酯。与mol.wt. 500-3000,具有分子量的短链脂族和/或芳族二醇。低于600,则为芳族环状和/或脂族二异氰酸酯。稳定剂,添加剂等。(II)是脂族和/或芳族环。二异氰酸酯和/或产生二异氰酸酯的cpd。和/或NCO封端的预聚物,其分子量为5000以下; (II)通过进料口或进料区或在挤出机或注塑机中的另一个合适位置以固体或液体形式添加到聚合物熔体中,或(II)在加工机外部与(III)预混合,然后照常处理湿润的颗粒。在加工或最终模制之后,将材料调理至少1(优选24)小时。在50-150(pref.100)摄氏度使用/优势-添加。 (II)的摩尔增加。 TPU的性能,使TPU弹性体具有更高的水解稳定性和耐磨性(适用于涂料,管材,型材,易损件等)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号