The high tensile compound material, which can withstand dynamic forces, has a matrix of mineral bonding and fibres of organic synthetic staple fibres with organic synthetic fibre dust. Netting is embedded into the matrix material mixture in layers. The organic synthetic fibres are pref. used at a rate of 2-5% of the bonding material mass, and the organic synthetic fibre dust is added at a rate of 5-10% of the bonding mass. The fibres have a length of 2-15mm and the fibre dust length is 0.05-2mm, and pref. 0.1-1.5mm. The fibres are pref. of polypropylene. The netting layers are of woven glass fibres, with a mesh width of 3-20mm in a material weight of 200-700 g/m2, for insertion into the matrix of bonding material and fibres. USE/ADVANTAGE - The material, especially based on plaster or cement, is used as plates or shaped bodies for new construction or restoration of dwellings, commercial property and industrial sites. The material, on bending forces, has a monolithic fracture behaviour, with the external forces transferred to the inner netting for strengt
机译:高强度复合材料可以承受动力,具有矿物粘合基质和有机合成短纤维纤维与有机合成纤维粉尘的基质。网被分层地嵌入基质材料混合物中。有机合成纤维是优选的。使用量为粘结材料质量的2-5%,有机合成纤维粉尘以粘结质量的5-10%的比例加入。纤维的长度为2-15mm,纤维粉尘的长度为0.05-2mm,优选。 0.1-1.5毫米。纤维是优选的。聚丙烯。所述网层是编织玻璃纤维,其网眼宽度为3-20mm,材料重量为200-700g / m 2,用于插入粘合材料和纤维的基质中。用途/优点-该材料(尤其是基于灰泥或水泥的材料)用作建筑或房屋,商业物业和工业场所的新建筑或修复的板材或成型体。材料在弯曲力作用下具有整体断裂特性,外力传递到内网以加强强度

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号