摘要

A pressureless sintering method is disclosed for use in the production of whisker-toughened ceramic composites wherein the sintered density of composites containing up to about 20 vol. % SiC whiskers is improved by reducing the average aspect ratio of the whiskers to from about 10 to about 20. Sintering aids further improve the density, permitting the production of composites containing 20 vol. % SiC with sintered densities of 94% or better of theoretical density by a pressureless sintering method.
机译:公开了一种用于生产晶须增韧的陶瓷复合材料的无压烧结方法,其中复合材料的烧结密度最高为约20体积%。通过将晶须的平均长径比从约10降低至约20来改善SiC晶须的%。烧结助剂进一步提高了密度,从而允许生产包含20vol。%的SiC的晶须。通过无压烧结法得到的烧结密度为理论密度的94%或更高的5%SiC。

著录项

  • 公开/公告号US5207958A

    专利类型

  • 公开/公告日1993-05-04

    原文格式PDF

  • 申请/专利权人 MARTIN MARIETTA ENERGY SYSTEMS INC.;

    申请/专利号US19910789390

  • 发明设计人 TERRY N. TIEGS;

    申请日1991-11-06

  • 分类号C04B35/10;

  • 国家 US

  • 入库时间 2022-08-22 04:58:25

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号