首页> 外国专利> CONTAMINATION PREVENTING METHOD FOR LAND STRUCTURE

CONTAMINATION PREVENTING METHOD FOR LAND STRUCTURE

机译:土地结构污染防治方法

摘要

PURPOSE: To prevent the adhesion of a contamination by applying a specified base coating on a land structure and drying and applying the coating containing a reactive curing type silicone resin on the base coating. ;CONSTITUTION: The base coating whose base resin is an epoxy resin and containing aminoalkoxy silane having ≥2 active hydrogen as a curing agent is applied on the land structure and dried. Then, the coating containing the reactive curing type silicone resin containing 50-99wt.% reactive curing type silicone resin and 1-50wt.% silicone resin expressed by the formula and having a hydroxyalkyl group or alkoxy group having 250-30000 number average mol.wt. and 20-50000 centistokes viscosity as a resin component is applied on the coated surface. In the formula, R is an aralkyl group, etc., R1 is a divalent aliphat. hydrocarbon group, R2 is hydrogen atom, etc., (x) and (y) is 0.01≤(x)≤3.99, 0.01≤(y)≤3.99, respectively and 0.02≤(x+y)≤4 is satisfied. In this way, the adhesion of a contamination is prevented over a long period.;COPYRIGHT: (C)1994,JPO&Japio
机译:目的:为了防止污染的粘附,可以在陆上结构上涂上规定的基础涂料,然后干燥,然后在基础涂料上涂上含有反应性固化型有机硅树脂的涂料。 ;组成:将基础树脂为环氧树脂,含有活性氢≥2的氨基烷氧基硅烷作为固化剂的基础涂料涂在陆基结构上并干燥。然后,包含含有反应性固化型有机硅树脂的涂料,所述反应性固化型有机硅树脂包含50-99wt。%的反应性固化型有机硅树脂和1-50wt。%的由所述式表示的并且具有数均摩尔数为250-30000的羟烷基或烷氧基。重量作为树脂成分的粘度为20〜50000厘s。式中,R为芳烷基等,R 1 为二价脂环。烃基,R 2 是氢原子等,(x)和(y)分别为0.01≤(x)≤3.99、0.01≤(y)≤3.99和0.02≤(x + y)≤4。这样,可以长期防止污染物的附着。;版权所有:(C)1994,日本特许厅&日本apio

著录项

  • 公开/公告号JPH06182290A

    专利类型

  • 公开/公告日1994-07-05

    原文格式PDF

  • 申请/专利权人 KANSAI PAINT CO LTD;

    申请/专利号JP19920355770

  • 发明设计人 OYA TSUTOMU;TANIGUCHI SHIGERU;

    申请日1992-12-18

  • 分类号B05D5/00;B05D7/00;B05D7/24;C09D5/00;C09D5/14;C09D163/00;C09D183/04;

  • 国家 JP

  • 入库时间 2022-08-22 04:48:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号