The present Invention refers to a procedure for the preparation of styrene butadiene Copolymer improved, which achieves fully incorporated,I.e. with zero nodes after mixed in a Roller Mill; characterised in that it comprises the polymerization reaction in Solution, styrene and butadiene.In a Hydrocarbon Solvent type, Solvent / COPOLYMER in a ratio of 5.4, with organolitiados Initiators in a ratio calculated for disable Poisons such as initial step and a concentration of 0.01 g per gram of initiator Agent aleatorizante tetrahydrofuran Copolymer, concentration of 0.66, Gram for gram of SiCl4 concentration preparation of Copolymer, in 0.0.007 g / g of Copolymer and initiating the Reaction at 30C and deactivated Aromatic Chains alive with alcohol at a concentration of 0.006 g / g of Copolymer.
机译:本发明涉及一种改进的苯乙烯丁二烯共聚物的制备方法,该方法可实现完全掺入。在辊磨机中混合后零节点;其特征在于它包括在溶液,苯乙烯和丁二烯中的聚合反应。在碳氢溶剂类型中,Solvent / COPOLYMER的比例为5.4,与有机锂引发剂的比例为禁用毒物(例如初始步骤)的浓度和0.01克每克引发剂Agent aleatorizante四氢呋喃共聚物每克,浓度为0.66克,在0.0.007克/克共聚物中的克数为SiCl4浓缩制剂,然后在30℃引发反应,并在一定浓度下用醇活化失活的芳香链0.006克/克共聚物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号