The nylon 6 fiber having excellent dyeing property and antistatic property is prepd. by add-mixing and reacting caprolactum, water and 0.3-10 mole% of the copolymonomer of formula R-(COOH)2 (I) and 2-15 wt.% of polyethylene glycol diamine at 230-280 deg.C for 5-12 hrs.; inputting and reacting a diamine of formula R'-(NH2)2 (II) of 13 times amt. w.r.t. amt. of the copolymonomer (I) at 250-280 deg.C for 20-30 hrs. and making a chip and extracting, drying; then solid-phase polymerizing that at 160-195 deg.C for 15-25 hrs. to form 2.40-2.70 viscosity (R.V) and 15-30 meq/kg of NH2 concentration of the solid-phase polymer; then melt-spinning that. In formulas, R is gp. of formula (1) or (2); R' is C2-C8 hydrocarbon gp. of formula (3), (4) or (5); M is Li, Na or K.
机译:准备具有优异的染色性和抗静电性的尼龙6纤维。通过将己内酯,水和0.3-10摩尔%的式R-(COOH)2(I)的共聚单体和2-15重量%的聚乙二醇二胺在230-280℃下添加混合并使之反应5- 12小时;输入13倍amt的式R′-(NH 2)2(II)的二胺并使之反应。 w.r.t. amt。共聚单体(I)在250-280℃下放置20-30小时。制成薄片并提取,干燥;然后在160-195℃固相聚合15-25小时。形成2.40-2.70粘度(R.V)和15-30 meq / kg的固相聚合物NH2浓度;然后将其熔融纺丝。式中,R为gp。具有式(1)或(2); R'是C2-C8烃gp。具有式(3),(4)或(5); M是Li,Na或K。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号