The method involves extruding a plastic strip at a temp. below a peroxide reaction temp. and initiating partial crosslinking. The strip is stretched at a temp. below the crystalline m.pt of the plastic. The strip is fully crosslinked during the heat shrinking stage. Pref. initial cross-linking involves using a mixture of peroxides, with different reaction temps. and times and can be initiated by irradiation, peroxide and/or silane. The degree of crosslinking can be varied by passing the plastic strip through a salt bath or steam and altering the passage time or temp.. The partially crosslinked strip is heated to a temp. below the crystalline m.pt. by passing through oil or heating with microwaves before stretching. Final crosslinking is achieved by heating the peroxide with microwaves and simultaneously cooling the surface. USE/ADVANTAGE - Producing heat shrinkable product, esp. for cable connectors or branches. Increased tear resistance and eased opening of shrink-wrapped component.
机译:该方法包括在一定温度下挤出塑料条。低于过氧化物反应温度并引发部分交联。该条带被临时拉伸。低于塑料的结晶熔点。该带在热收缩阶段被完全交联。首选初始交联涉及使用具有不同反应温度的过氧化物混合物。和时间,可以通过辐射,过氧化物和/或硅烷引发。可以通过使塑料条通过盐浴或蒸汽并改变通过时间或温度来改变交联度。将部分交联的条加热至温度。低于结晶熔点在拉伸前先通过油或用微波加热。通过用微波加热过氧化物并同时冷却表面来实现最终的交联。使用/优点-生产热收缩产品,尤其是。用于电缆连接器或分支。提高了抗撕裂性,并减轻了收缩包裹部件的开口。

著录项

相似文献

  • 专利
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号