PURPOSE:To easily coat the surface of a base material with the bioactive apatite film resembling in-vivo bones without subjecting the base material to a heating treatment by disposing the base material and glass to face each other and immersing the same into an aq. hydroxylapatite component soln. of satd. and supersatd. concns. CONSTITUTION:The base material and the glass essentially consisting of CaO and SiO2 are disposed to face each other at a spacing of a specified distance or below and are immersed into the aq. hydroxylapatite component soln. of the satd. and supersatd. concns., by which the film of the hydroxylapatite resembling to the bones is formed on the surface of the base material. The compsn. of the glass to be opposed to the base material, the ion concn., pH and temp. of the aq. soln. in which the base material is immersed, and further, the spacing between the base material and the glass are preferably limited respectively within prescribed ranges in order to efficiently execute the above-mentioned coating method. The glass to be used is preferably composed of 20 to 60% CaO, 40 to 80mol% SiO2 and =70mol% total of the CaO and the SiO2.
机译:用途:通过将基材和玻璃相互面对并将其浸入水溶液中,从而轻松地在基材表面上覆盖类似于骨骼的生物活性磷灰石膜,而无需对基材进行热处理。羟磷灰石组分溶液。的和超级。 conns。组成:基本材料和主要由CaO和SiO2组成的玻璃以相对于指定距离或以下的间距相对放置,并浸入水溶液中。羟磷灰石组分溶液。饱和的和超级。因此,在基体材料的表面上形成类似于骨头的羟磷灰石膜。该compsn。与基材相对的玻璃的离子浓度,pH和温度。的水soln。另外,为了有效地进行上述涂布方法,优选将基材和玻璃的间隔分别限制在规定的范围内。所使用的玻璃优选由20至60%的CaO,40至80摩尔%的SiO 2以及CaO和SiO 2的总和≥70摩尔%组成。

著录项

  • 公开/公告号DE68908158T2

    专利类型

  • 公开/公告日1993-11-25

    原文格式PDF

  • 申请/专利权人 UNIV KYOTO JP;

    申请/专利号DE1989608158T

  • 申请日1989-11-10

  • 分类号A61L27/00;B05D1/18;

  • 国家 DE

  • 入库时间 2022-08-22 04:35:23

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号