Method of preparation of bitumen - polymer compositions, the application of the compositions obtained in the embodiment of a coatings and of the polymer solution for obtaining said compositions.

机译:沥青-聚合物组合物的制备方法,在涂料的实施方案中获得的组合物的应用以及用于获得所述组合物的聚合物溶液的应用。

摘要

A process is provided for the preparation of a bitumen-polymer composition which comprises (a) producing at a temperature of between 100 DEG C. and 230 DEG C., a mixture of (i) a bitumen; (ii) a linear block copolymer of styrene and a conjugated diene, the block copolymer being used in a quantity of from 0.5% to 25% by weight of bitumen and having a weight-average molecular weight of between 170,00 and 250,000 and a structure of A-B with A denoting a polymer block consisting of a polystyrene block which may be extended on the B side by a random copolymer of styrene and of the conjugated. diene and B denoting a polymer block consisting of conjugated diene units, and (iii) a coupling agent containing at least one sulphur-donor compound and used in an amount to provide a quantity of sulphur representing, by weight, 0.1% to 10% of the weight of the liner block copolymer of styrene and conjugated diene; and (b) keeping the mixture thus produced at a temperature of between 100 DEG C. and 230 DEG C. and with stirring, for a period of at least ten minutes.
机译:提供了一种制备沥青聚合物组合物的方法,该方法包括:(a)在100℃至230℃的温度下生产(i)沥青的混合物; (ii)苯乙烯和共轭二烯的线性嵌段共聚物,该嵌段共聚物的用量为沥青的0.5重量%至25重量%,并且重均分子量为170,00至250,000之间,并且AB的结构,其中A表示由聚苯乙烯嵌段组成的聚合物嵌段,该聚苯乙烯嵌段可以通过苯乙烯和共轭的无规共聚物在B侧延伸。二烯和B表示由共轭二烯单元组成的聚合物嵌段,以及(iii)包含至少一种硫供体化合物的偶联剂,其用量为提供一定量的硫,按重量计占0.1%至10%苯乙烯和共轭二烯的衬里嵌段共聚物的重量; (b)将如此制得的混合物在100℃至230℃的温度下保持搅拌至少十分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号