首页> 外国专利> Method of manufacturing a color CRT to optimize the magnetic performance

Method of manufacturing a color CRT to optimize the magnetic performance

机译:制造彩色CRT以优化磁性能的方法

摘要

The magnetic performance of a color CRT is optimized by firing ferromagnetic components thereof in an exothermic atmosphere to anneal the components and form a stable black iron oxide layer on a surface thereof. The components are introduced into a furnace having such an atmosphere and the components are heated to a temperature sufficient to initiate pre-oxidation of the surface thereof. The temperature is then increased to optimize the magnetic characteristics of the components and at least partially relieve stress therein. The components are next cooled to a temperature at which the thickness of the stable black oxide layer on the surface of the components is optimized. A CRT is manufactured according to the process described above.
机译:彩色CRT的磁性能是通过在放热气氛中烧成其铁磁成分以使其退火并在其表面上形成稳定的黑色氧化铁层来优化的。将组分引入具有这种气氛的炉中,并将组分加热至足以引发其表面的预氧化的温度。然后升高温度以优化部件的磁特性并至少部分缓解部件中的应力。接下来将部件冷却至使部件表面上的稳定的黑色氧化物层的厚度最优化的温度。根据上述方法制造CRT。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号