Method for starting continuous casting in continuous slab casting and method for setting a dummy bar prior to the start of casting of continuous slab casting

机译:在连续板坯连铸中开始连续铸造的方法和在开始进行连续板坯连铸之前设置铸坯的方法

摘要

A method for starting continuous slab casting capable of facilitating withdrawal of a dummy bar to start smooth continuous slab casting is provided at the start of casting of continuous slab casting, where lateral side plates 2 of the mold 10 are pinched by longitudinal side plates 1 of the mold and are adjustable in the slab width direction; where a dummy bar 4 is set at a desired level at the center in a width- variable, continuous casting mold; and clearances each between lateral side plates 2 and the dummy bar 4 are adjusted to 1-3 mm, while maintaining the lateral side plates 2 vertically, then sealing materials 5 are filled into the clearances; then molten steel is poured into the mold; and then the top ends of the lateral side plates 2 are made more apart outwardly, thereby giving a downwardly tapered profile to the lateral side plates 2, when no more poured molten steel is passed into the clearance between the formed solidified shell 6a and the plates 1 and 2, while withdrawing the dummy bar 4 downwardly; whereby the continuous slab casting is conducted.
机译:在开始进行连续板坯铸造的过程中,提供了一种开始进行连续板坯铸造的方法,该方法能够促进空心棒的拔出,从而开始平滑的连续板坯铸造,其中,模具10的横向侧板2被模具10的纵向侧板1挤压。模具,可沿板坯宽度方向调节;在宽度可变的连续铸造模具中,在中间将虚设棒4设置在期望的水平;将侧板2与虚设杆4之间的间隙调整为1〜3mm,同时将侧板2保持为垂直状态,然后在该间隙中填充密封材料5。然后将钢水倒入模具中。然后,当不再有浇注的钢水进入所形成的凝固壳体6a和板之间的间隙时,使侧板2的顶端向外更分开,从而使侧板2具有向下的锥形轮廓。参照图1和图2,同时向下拉出伪杆4;从而进行连续的板坯铸造。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号