首页> 外国专利> PHASE DIFFERENCE FILM AND METHOD FOR REGULATING WAVELENGTH DEPENDENCE OF PHASE DIFFERENCE FILM

PHASE DIFFERENCE FILM AND METHOD FOR REGULATING WAVELENGTH DEPENDENCE OF PHASE DIFFERENCE FILM

机译:相位差膜和调节相位差膜的波长相关性的方法

摘要

PURPOSE: To obtain an inexpensive phase difference film in which wavelength dependence is easily regulated without requiring a complicated process by incorporating a plasticizer into a thermoplastic resin. ;CONSTITUTION: This phase difference film consists of 100 pts.wt. thermoplastic resin and 2-20 pts.wt. plasticizer. The plasticizer, to be used is, for example, phthalic acid-base plasticizer such as dimethylphthalate and diethylphthalate, aliphatic dibasic acid-base plasticizer such as adipic acid-2-ethylhexyl and adipic acid-di-n-decyl, phosphate-base plasticizer such as tributhylphosphate and tri-2- ethylhexylphosphate, and epoxy plasticizer such as epoxidized soybean oil and epoxydized talleol fatty acid 2-ethylhexyl. It is preferable to use a polymer plasticizer such as polyester-base or polyether-base one at the standpoint that the polymer has small transfer property.;COPYRIGHT: (C)1995,JPO
机译:用途:通过将增塑剂掺入热塑性树脂中,获得一种廉价的相位差膜,该膜中的波长依赖性易于调节,而无需复杂的过程。 ;组成:此相差薄膜由100 pts.wt组成。热塑性树脂和2-20 pts.wt.增塑剂。作为增塑剂,可以使用例如邻苯二甲酸二甲酯,邻苯二甲酸二乙酯等邻苯二甲酸系增塑剂,己二酸-2-乙基己基己二酸,己二酸二正癸基等脂肪族二元酸系增塑剂,磷酸盐系增塑剂等。例如磷酸三丁酯和磷酸三-2-乙基己基酯,以及环氧增塑剂,例如环氧化大豆油和环氧化塔耳醇脂肪酸2-乙基己基。从聚合物具有小的转移性能的角度出发,优选使用聚合物增塑剂,例如聚酯基或聚醚基。COPYRIGHT:(C)1995,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号