WELDING WIRE AND WELDING METHOD FOR PREHEATING TEMPERATURE DECREASING HIGH TENSILE STEEL

机译:预热降低高强度钢的焊接线和焊接方法

摘要

PURPOSE: To provide a welding wire and welding method by which defectless weld metal can be obtained by suppressing preheating to be executed prior to welding at a temp. lower than the temp. at which the preheating is executed heretofore in the case of using of a wire having the equiv. strength in welding to be applied to high-strength steel products. ;CONSTITUTION: This welding wire contains 0.03 to 0.1% C, 0.3 to 1.0% Si, 0.9 to 2.5& Mn, 0.1 to 0.6% Mo and 0.05 to 0.5% Cu and one or two kinds of 0.05 to 0.20% V and 0.01 to 0.3% Nb. Further, 0.3 to 2.5% Ni, 0.1 to 0.5% Cr, 0.05 to 0.35% Ti and 0.0005 to 0.0080% B are incorporated therein. Welding working efficiency and working environment are improved by using this wire.;COPYRIGHT: (C)1995,JPO
机译:目的:提供一种焊丝和焊接方法,通过抑制在进行临时焊接之前执行的预热,可以获得无缺陷的焊接金属。低于温度在使用具有等价线的情况下,在此之前执行预热。适用于高强度钢材的焊接强度。 ;组成:该焊丝包含0.03至0.1%C,0.3至1.0%Si,0.9至2.5&Mn,0.1至0.6%Mo和0.05至0.5%Cu和一种或两种0.05至0.20%V和0.01至0.01% 0.3%铌此外,其中掺入0.3至2.5%的Ni,0.1至0.5%的Cr,0.05至0.35%的Ti和0.0005至0.0080%的B。使用该焊丝可提高焊接工作效率和工作环境。版权所有:(日本)JPO(C)1995

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号