Polyurethane foams having improved retention of insulative properties can be prepared using one or more of two novel polyols. One of the polyols is a polyether prepared by reacting a monoepoxide with a compound having the general formula: ##STR1## wherein X is H, Li, Na, K; A is N, S or O; L is a covalent bond or a connecting group having from 1 to 10 carbons; M is any group capable of reacting with an ethylene oxide molecule in the presence of a basic catalyst; and J is an integer from 2 to 8. The other polyol is prepared by (1) admixing ethylene carbonate and one or more hydroxyl functional compounds under reaction conditions sufficient to react the ethylene carbonate and the hydroxyl functional compounds to produce a polyol precursor, and (2) admixing the polyol precursor with diethylene glycol and an anhydride, a dicarboxylic acid, a tricarboxylic acid or mixtures thereof, optionally in the presence of a catalyst.
机译:可以使用两种新型多元醇中的一种或多种来制备具有改善的绝缘性保持性的聚氨酯泡沫。一种多元醇是通过使单环氧化物与具有以下通式的化合物反应制备的聚醚:其中X是H,Li,Na,K;和A是N,S或O; L为共价键或具有1至10个碳的连接基团; M是在碱性催化剂的存在下能够与环氧乙烷分子反应的任何基团; J为2〜8的整数。(1)在足以使碳酸亚乙酯与羟基官能化合物反应生成多元醇前体的反应条件下,将碳酸亚乙酯与一种或多种羟基官能化合物混合而制备其他多元醇。 (2)任选地在催化剂的存在下,将多元醇前体与二甘醇和酸酐,二羧酸,三羧酸或其混合物混合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号