Disclosed herein is a poly(arylene thioether-ketone-ketone) copolymer comprising (A) at least one poly(arylene thioether-ketone- ketone) segment having predominant recurring units of the formula ##STR1## and (B) at least one poly(arylene thioether) segment having predominant recurring units of the formula ##STR2## (a) the ratio of the total amount of the poly(arylene thioether) segment (B) to the total amount of the poly(arylene thioether-ketone-ketone) segment (A) ranging from 0.1 to 9 by weight, (b) the weight-average molecular weight of the poly(arylene thioether) segment (B) being at least 200 but lower than 1000, and (c) said copolymer having a melt viscosity of 2-100,000 poises as measured at 380 C. and a shear rate of 1,200/sec as well as a production process of the poly(arylene thioether-ketone-ketone) copolymer. The copolymer has high crystallinity and heat resistance, uniform composition, and excellent melt stability, processability, handling properties, solvent resistance and moisture absorption resistance.
机译:本文公开了一种聚(亚芳基硫醚-酮-酮)共聚物,其包含(A)至少一个具有式## STR1 ##的主要重复单元的聚(亚芳基硫醚-酮-酮)链段和(B)至少一个具有式## STR2 ##的主要重复单元的聚(亚芳基硫醚)链段(a)聚(亚芳基硫醚)链段(B)的总量与聚(亚芳基硫醚醚)的总量之比-酮)链段(A)的重量比为0.1至9,(b)聚(亚芳基硫醚)链段(B)的重均分子量至少为200但小于1000,并且(c)所述共聚物在380℃下测得的熔体粘度为2-100,000泊泊,剪切速率为1200 /秒,以及聚(亚芳基硫醚-酮-酮)共聚物的生产方法。该共聚物具有高结晶度和耐热性,均匀的组成以及优异的熔体稳定性,可加工性,处理性能,耐溶剂性和耐吸湿性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号