A pulp with ph=9.5 to 11.5, resin, and cyanide KCN is fed to a reaction zone. KCN is in a concentration of CN.sup.- ions in the liquid phase of the pulp from about 0.1 to about 10 g/l, which is maintained constant. The sorbent is in an amount providing its concentration 1 to 1. 5% of the reaction zone volume. The leaching procedure produces a sorbent with impurities and rich in gold and silver, and a cyanic pulp depleted of gold and silver. Then, the sorbent rich in gold and silver is separated from the cyanic pulp. The saturated sorbent with impurities is processed in the desorption zone in two stages by passing therethrough a sulfuric acid solution of thiourea, the volume of the solution comprising 10 to 15 volumes of said sorbent. The sulfuric acid solution of thiourea is in an amount of 30% to 50% of said solution volume. A sulfuric acid solution of thiourea rich in gold and silver and a sorbent depleted of gold, silver and impurities is obtained. The remaining amount of the sulfuric acid solution of thiourea is fed onto the sorbent depleted of gold, silver and impurities to obtain a sulfuric acid solution of thiourea depleted of gold and silver, which is supplied to the first processing stage, and a sorbent with a residual content of gold, silver and impurities.
机译:将具有ph = 9.5至11.5的纸浆,树脂和氰化物KCN送入反应区。 KCN在纸浆液相中的CNs浓度约为0.1至10 g / l,保持恒定。吸附剂的量应使其浓度为反应区体积的1-1.5%。浸出过程产生的杂质吸附剂中含有丰富的金和银,而氰化纸浆则消耗了金和银。然后,将富含金和银的吸附剂与氰化浆分离。通过使硫脲的硫酸溶液从中通过,使具有杂质的饱和吸附剂在解吸区中分两个阶段进行处理,该溶液的体积包括10至15体积的所述吸附剂。硫脲的硫酸溶液的量为所述溶液体积的30%至50%。获得了富含金和银的硫脲的硫酸溶液以及贫化了金,银和杂质的吸附剂。将剩余量的硫脲硫酸溶液进料到贫化了金,银和杂质的吸附剂上,从而得到了贫化了金和银的硫脲硫酸溶液,将其供应到第一处理阶段,并用金,银和杂质的残留量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号