Process for the preservation of wood and wood materials and the use of a polymeric, quaternary ammonium borate for temporary blistering protection and for preventive wood protection
Process for the preservation of wood and wood materials and the use of a polymeric, quaternary ammonium borate for temporary blistering protection and for preventive wood protection
展开▼
机译:木材和木质材料的保存方法以及使用聚合的季铵硼酸盐进行临时起泡保护和预防性木材保护的方法
展开▼
页面导航
摘要
著录项
摘要
A biocidal preservative for cellulose-containing products containing a biocidally effective amount of a polymeric quaternary ammonium borate obtained by simultaneous reaction of (A) at least one member of the group consisting of boric acid and salts and esters thereof and (B) an amine of the formula IMAGE and (C) ethylene oxide or propylene oxide wherein R1 is alkyl or alkenyl of 8 to 22 carbon atoms and R2 is hydrogen, alkyl of 1 to 22 carbon atoms or -CH2CH2NH2 or R1 is alkyl of 1 to 4 carbon atoms and R2 is -(CH2CH2O)x-H or -(CH2CH2CH2O)x-H, R3 is selected from the group consisting of hydrogen, -(CH2CH2O)x-H, (CH2CH2CH2O)x-H and -CH2CH2CH2NH2, R4 and R6 are individually selected from the group consisting of alkyl of 1 to 4 carbon atoms, -(CH2CH2O)x-H and -(CH2CH2CH2O)x-H, and R5 and R7 are individually -(CH2CH2O)x-H and -(CH2CH2CH2O)x-H, A is selected from the group consisting of -(CH2)n, -(CH2CH2-O-CH2CH2)n- and -(CH2CH2-NH-CH2CH2)n-x is an integer from 1 to 55 and n is an integer of 1 to 20, the molar ratio of A:B:C being 1:2 to 20:0.6 to 1.5.
展开▼