nodular cast iron and nodular cast iron, the cast iron process to obtain nodular including: a metal plate martensite, bainiteperlitica or ferrite having a purity of about 99.6% in which the content of sulfur and phosphorus are maintained below 0.015% and 0.04%, respectively, from 10 to 12% by volume of graphite particles and from about 0.2 to 1.2% by volume of particles of the carbide of high hardness of mc.these particles are dispersed in the molten metal matrix, where m is at least one of the elements selected from the group consisting of ti, ta. zr, hf, v, and nb.the invention also concerns a process for nodular iron comprising the phases of: adding to a bath of grey cast iron containing less than 0.015% sulphur and less than 0.04% of phosphorus, a load between about 0.2 and 1.2% reported on weight of bath of at least one area having the formula fe - fe - fem and mc.where m is at least one of the elements selected from the group consisting of ti, ta, zr, hf,v and nb; carrying out at least one nodulizzazione of bathroom by inoculation of magnesium at low content of ferrosilicon in it; and passing the metal bath in the mold nodulizzato (fig. 2).
机译:球墨铸铁和球墨铸铁,获得球墨铸铁的工艺包括:纯度约为99.6%的金属板马氏体,贝氏体或铁素体,其中硫和磷的含量分别保持在0.015%和0.04%以下含有10至12体积%的石墨颗粒和约0.2至1.2体积%的具有mc高硬度的碳化物,这些颗粒分散在熔融金属基体中,其中m是至少一种元素选自ti,ta。 zr,hf,v和nb。本发明还涉及球墨铸铁的工艺,该工艺包括以下阶段:向含灰量小于0.015%且磷小于0.04%的灰铸铁浴中加入约0.2的负载。至少有一个化学式为fe-fe-fem和mc的区域占浴重的1.2%,其中m为选自ti,ta,zr,hf,v和nb的至少一种元素;通过在浴室中接种低含量的硅铁来进行至少一个结核菌根瘤的治疗;然后将金属熔池通过模具中的nodulizzato(图2)。

著录项

  • 公开/公告号IT1263941B

    专利类型

  • 公开/公告日1996-09-05

    原文格式PDF

  • 申请/专利权人

    申请/专利号IT1993MI00305

  • 发明设计人

    申请日1993-02-18

  • 分类号6C21BA;

  • 国家 IT

  • 入库时间 2022-08-22 03:52:09

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号