Manufacturing method of polyester yarn by high speed spinning

机译:高速纺制涤纶纱的方法

摘要

The present invention by installing a heating pipe for heat treatment during the production of polyester yarn by a high-speed spinning method of more than 5,000m / min spinning speed in two stages to reduce the radiation tension and increase the elongation to prevent the occurrence of shear and trimming It is to be able to produce a polyester yarn of excellent quality, which is composed of a heating pipe divided into two stages, the first stage of the internal heating temperature to 120-140 ℃ and the length of 50-80 ㎝, The second stage consists of internal heating temperature of 180-200 ℃ and length of 80-100cm.
机译:本发明通过以大于5,000m / min的纺丝速度的高速纺纱方法在两个阶段中安装聚酯制丝过程中用于热处理的加热管,以降低辐射张力并增加伸长率以防止发生纺丝。剪切和修整为了能够生产出高质量的涤纶纱,它由分为两个阶段的加热管组成,第一阶段的内部加热温度为120-140℃,长度为50-80㎝ ,第二阶段包括内部加热温度为180-200℃,长度为80-100cm。

著录项

  • 公开/公告号KR960010913A

    专利类型

  • 公开/公告日1996-04-20

    原文格式PDF

  • 申请/专利权人 김준웅;

    申请/专利号KR19940023162

  • 发明设计人 심성영;오영수;최영근;

    申请日1994-09-14

  • 分类号D01D5/084;

  • 国家 KR

  • 入库时间 2022-08-22 03:45:20

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号