PURPOSE: To crush waste brick from a metal melting furnace simply to a small particle size by crushing the brick which is brought into contact with steam of specified pressure or more. ;CONSTITUTION: Base resisting refractory brick used in a metal melting furnace contains MgO and/or CaO as main components, and magnesium chloride brick and magnesia brick are used more preferably. Since MgO and CaO are reactive in a hydration reaction with water, waste brick from the furnace is brought into contact with steam of 2atm or more to be crushed. The temperature of steam is preferably 100-310°C and more preferably 150-250°C. The temperatures are reduced into saturated steam pressure to be 1.0-100atm. and more preferably 4.9-40atm. The treatment with steam is preferably carried out in an autoclave. The crushed waste brick is preferably melted in a copper melting furnace.;COPYRIGHT: (C)1996,JPO
机译:目的:通过粉碎与指定压力或更高压力的蒸汽接触的砖,将金属熔化炉中的废砖粉碎成小颗粒。组成:金属熔炼炉中使用的耐碱耐火砖以MgO和/或CaO为主要成分,更优选使用氯化镁砖和氧化镁砖。由于MgO和CaO在与水的水合反应中是反应性的,因此使来自炉的废砖与2atm或更高的蒸汽接触以被粉碎。蒸汽的温度优选为100-310℃,更优选为150-250℃。将温度降低至饱和蒸汽压至1.0-100atm。更优选4.9-40atm。蒸汽处理优选在高压釜中进行。压碎的废砖优选在铜熔化炉中熔化。;版权所有:(C)1996,日本特许厅

著录项

  • 公开/公告号JPH08299835A

    专利类型

  • 公开/公告日1996-11-19

    原文格式PDF

  • 申请/专利权人 NIKKO KINZOKU KK;

    申请/专利号JP19950111402

  • 申请日1995-05-10

  • 分类号B02C19/18;B09B3/00;C22B7/00;

  • 国家 JP

  • 入库时间 2022-08-22 03:35:32

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号