PROBLEM TO BE SOLVED: To provide an Ag matrix which is excellent in welding resistance and whose contact resistance is low, and provide a contact material having the long sevice life. SOLUTION: An Ag solid solution where Sn of 5 to 10wt.% and Bi of 0.3 to 1.5wt.% are brought into solid solution in Ag, is internally oxidized at a temperature not less than its melting point, and is actualized as SnO2 of 4.1 to 11.9wt.%, Sn2 Bi2 O7 of 1.1 to 5.3wt.% Bi2 O3 not more than 0.01wt.%, and SnO2 and Sn2 Bi2 O7 are dispersed as a spherical body having an average particle diameter of 0.1 to 0.7m, and a residual part is obtained as Ag, and an electric contact material is obtained. Next, a clad rivet contact point whose surface layer is composed of the electric contact material and base layer is formed as a two-layer to three-layer clad being Cu or Cu alloy is obtained, or a clad cross bar contact formed as a two-layer to five-layer clad is obtained. Next, an automobile relay and a television power supply relay are obtained which uses the clad rivet contact and the clad cross bar contact as an electric contactor.
机译:解决的问题:提供一种Ag基体,该Ag基体具有优异的焊接电阻并且其接触电阻低,并且提供了具有长使用寿命的接触材料。溶液:一种Ag固溶体,其中将5-10wt。%的Sn和0.3-1.5wt。%的Bi引入Ag的固溶体,并在不低于其熔点的温度下内部氧化,并实现为SnO2将4.1〜11.9wt。%,Sn 2 Bi 2 O 7为1.1〜5.3wt。%的Bi 2 O 3不超过0.01wt。%,将SnO 2和Sn 2 Bi 2 O 7分散为平均粒径为0.1〜0.7m的球形。获得残余部分作为Ag,并获得电接触材料。接下来,获得其表面层由电接触材料构成并且基层形成为Cu或Cu合金的两层至三层包层的包层铆钉接触点,或者获得形成为两层的包层交叉棒触点。获得五层到五层的包层。接着,获得使用包层铆钉触点和包层横杆触点作为电接触器的汽车继电器和电视电源继电器。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号