PROBLEM TO BE SOLVED: To enhance dispersability by opening non-asbestos fibers used when a joint sheet is molded by kneading non-asbestos fibers along with a rubber binder, a vulcanizing agent and a filler by using an opening machine. ;SOLUTION: When a joint sheet is produced, at first, opened non-asbestos fibers 1B obtained by opening non-asbestos fibers 1 by an opening machine 1A such as an Eirich mixer, a Loedige mixer or an impact grinder, a rubber binder 2, a vulcanizing agent 3 and a filler 4 are kneaded by a kneader in a first step A and the kneaded mixture is aged in a second step B and weighed in a thirst step C. Subsequently, the kneaded mixture is molded into the joint sheet in a fourth step D and the joint sheet is finally finished in a fifth step E. Since non-asbestos fibers 1 are opened by the opening machine 1A to be kneaded as opened non-asbestos fibers 1B, dispersibility at a time of kneading is good and the high tensile strength by uniform dispersion can be obtained.;COPYRIGHT: (C)1997,JPO
机译:要解决的问题:通过打开非石棉纤维来提高分散性,该非石棉纤维是通过使用开松机将非石棉纤维与橡胶粘合剂,硫化剂和填料捏合而模制成接缝片而制成的。 ;解决方案:生产接缝片时,首先,要打开无石棉纤维1B,该纤维是通过开松机1A(例如Eirich混合机,Loedige混合机或冲击式研磨机,橡胶粘合剂2)将非石棉纤维1开松而获得的在第一步骤A中,通过捏合机捏合硫化剂3和填充剂4,并且在第二步骤B中将捏合的混合物老化,并在干渴的步骤C中称重。随后,将捏合的混合物成型为接缝片。第四工序D,最后在第五工序E中完成接缝片材。由于通过开松机1A将非石棉纤维1打开,作为开松的非石棉纤维1B进行混炼,因此混炼时的分散性良好,并且通过均匀分散可以获得较高的拉伸强度。版权所有:(C)1997,日本特许厅

著录项

  • 公开/公告号JPH0929082A

    专利类型

  • 公开/公告日1997-02-04

    原文格式PDF

  • 申请/专利权人 ASK TEKUNIKA:KK;

    申请/专利号JP19950187364

  • 申请日1995-07-24

  • 分类号B01F3/18;

  • 国家 JP

  • 入库时间 2022-08-22 03:33:47

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号