According to the invention, this is a reinforcing fiber ceramic Type not rust or carbon for the manufacture of a composite material of glass matrix, ceramic or ceramic by a process comprising the steps of: IF NECESSARY, oxidise FIBER SURFACE OR PUT IN A LAYER OF IT BUT same composition comprising oxygen; INTRODUCING THE FIBER IN A deposition chamber CHEMICAL VAPOR; PERFORM PRETREATMENT at a temperature of 850 to 1250 (DEGREES) C under hydrogen at a pressure of 50 to 300 mbar; Injecting a mixture of carrier gas NEUTRAL AND AMMONIA; STOPPING THE INJECTION AND REGULAR PRESSURE TO A value of 1 to 10 mbar; INJECT AICI3 IN A GAS SOLVENT NEUTRAL; MAKE A DEPOSIT IN FIBER AIN SIMULTANEOUS INJECTION OF A MIXTURE OF GAS AND CARRIER AICI3 NEUTRAL AND A MIXTURE OF NH3 AND GAS PRODUCING CARRIER NEUTRAL TO THE DESIRED THICKNESS AIN; After stopping the injection, cooled to a gas stream NEUTROY RECOVER THE FIBER. APPLICATION IN THE MANUFACTURE COMPOSITE having good oxidation resistance.
机译:根据本发明,这是一种不锈或碳的增强纤维陶瓷,用于通过以下方法制造玻璃基体,陶瓷或陶瓷的复合材料,该方法包括以下步骤:必要时,氧化纤维表面或将其置于层中IT B但包含氧气的相同组成;将纤维引入沉积室化学蒸气中;在氢气和50至300毫巴的压力下于850至1250(摄氏度)的温度下进行预处理;注入载气中性和氨的混合物;将注射和常规压力停止在1到10 mbar的值;在气体中性溶剂中注射AICI3;在纤维内沉积同时注入气体和载体AICI3中性混合物,以及将NH3和气体产生中性混合物至所需厚度内。停止注射后,冷却至气流NEUTROY RECOVER FIBER。在具有良好的抗氧化性的制造复合材料中的应用。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号