首页> 外国专利> Artificial lightweight aggregate containing a large amount of fly ash and its manufacturing method

Artificial lightweight aggregate containing a large amount of fly ash and its manufacturing method

机译:含有大量粉煤灰的人造轻质骨料及其制造方法

摘要

The present invention relates to a lightweight aggregate consisting of 40 to 90% by weight of fly ash and 10 to 60% by weight of shale and a manufacturing method thereof. According to the present invention, the fly ash 40 to 90% by weight, the SiO 2 content is 55% by weight or less and the total content of CaO, MgO, Na 2 O, K 2 O and FeO 10 to 60% by weight of shale Kneading and granulation by adding water to the% consists of firing at 1140 ~ 1355 ℃ in the air or in a reducing atmosphere.
机译:本发明涉及由40至90重量%的飞灰和10至60重量%的页岩组成的轻质骨料及其制造方法。根据本发明,粉煤灰为40-90重量%,SiO 2 含量为55重量%以下,并且CaO,MgO,Na 2 O,K 2 O和FeO页岩重量的10%到60%(通过在其中添加水进行捏合和制粒)包括在空气中或还原性气氛中于1140〜1355℃烧成。

著录项

  • 公开/公告号KR970026983A

    专利类型

  • 公开/公告日1997-06-24

    原文格式PDF

  • 申请/专利权人 이현구;

    申请/专利号KR19950042489

  • 发明设计人 이현구;정현희;박영훈;전영석;

    申请日1995-11-21

  • 分类号C04B18/10;

  • 国家 KR

  • 入库时间 2022-08-22 03:17:33