首页> 外国专利> Titanium addition to a water tube adjacent to a soot blower of a pulverized coal boiler Amorphous transition metal film treatment

Titanium addition to a water tube adjacent to a soot blower of a pulverized coal boiler Amorphous transition metal film treatment

机译:除粉煤锅炉烟灰鼓风机水管外还添加了钛非晶态过渡金属膜处理

摘要

The water pipe adjacent to the coal-fired boiler of the large coal-fired power plant was rubbed with an iron brush and wiped clean with solvent. Then, 20-30 mesh alumina was sprayed by a grit blasting machine to form irregularities. Then, 1.1-2.4 wt% of Si and 24.5-32.0 wt% %, Mn 1.0-2.8 wt%, B 3.0-4.2 wt%, Ti 0.15-0.65 wt%, Fe 57.73-70.25 wt%, C 0-0.2 wt% and S 0-0.02 wt% Or HVOF spraying method, it is possible to apply the coating of 0.25-0.75mm in thickness to improve the hardness, increase the hardness, and protect the water tube from erosion in the long term by the strong adhesive force, excellent thermal shock resistance,
机译:用铁刷摩擦大型燃煤电厂燃煤锅炉附近的水管,并用溶剂擦拭干净。然后,用喷砂机喷洒20-30目氧化铝以形成不规则形状。然后,Si的1.1-2.4wt%和24.5-32.0wt%,Mn 1.0-2.8wt%,B 3.0-4.2wt%,Ti 0.15-0.65wt%,Fe 57.73-70.25wt%,C 0-0.2wt%。 %和S 0-0.02 wt%或HVOF喷涂方法,可以通过施加0.25-0.75mm的厚度来提高硬度,增加硬度并长期保护水管不受强腐蚀的影响附着力,优异的抗热震性,

著录项

  • 公开/公告号KR970062060A

    专利类型

  • 公开/公告日1997-09-12

    原文格式PDF

  • 申请/专利权人 김병두;

    申请/专利号KR19960003005

  • 发明设计人 김병두;

    申请日1996-02-08

  • 分类号C23C4/04;

  • 国家 KR

  • 入库时间 2022-08-22 03:16:23

获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号