FIELD: polymerization of ethylene and copolymerization of ethylene with -olefins. SUBSTANCE: desired solid component contains product of consequent dissolution of tetra-C2-C4-alkoxy titanium and magnesium chloride in ethyl acetate, molar ratio of tetra-C2-C4-alkoxy titanium and magnesium chloride is 0.99: 1.00 respectively. Then activated silica gel is impregnated with thus prepared solution, ethyl acetate is evaporated at temperatures up to 60 C. Solid residue is treated by solution of aluminium ethyl sesquichloride in inert hydrocarbon to isolate solid product which comprises 1.4-2.2 gram-atom of magnesium, 5.3-7.5 gram-atom of chlorine and 0.4-0.7 butoxy groups per 1 gram-atom of titanium. Said treatment is carried out within 15 min at 25 C, it is followed by isolation and washing of desired product. EFFECT: improves quality of desired product, improves efficiency of the method. 9 cl
机译:领域:乙烯的聚合和乙烯与-烯烃的共聚。物质:所需的固体成分包含随后将四-C 2 -C 4 -烷氧基钛和氯化镁溶解在乙酸乙酯中的产物,四-C 2 -C 4 -烷氧基钛和氯化镁分别为0.99:1.00。然后用如此制备的溶液浸渍活化的硅胶,在高达60℃的温度下蒸发乙酸乙酯。通过倍半氯化铝乙基铝在惰性烃中的溶液处理固体残余物,以分离出包含1.4-2.2克原子的镁的固体产物,每1克原子的钛有5.3-7.5克原子的氯和0.4-0.7丁氧基。所述处理在25℃下在15分钟内进行,然后分离并洗涤所需产物。效果:提高所需产品的质量,提高方法的效率。 9厘升

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号