FIELD: marking pavement. SUBSTANCE: marking pavement is carried out by melting of thermoplastic composition. Said composition comprises block copolymer having common formula (A-B)n-A or (A-B)n+1X where A is preferably poly(conjugated vinyl aromatic) block; B is preferably poly(conjugated diene) block; X is residue of polyvalent cross-linking agent; n is integer from 1 to 3. Block A are 8-50 mass % of weight of said block copolymer, total molecular weight of block copolymer being 20000-50000, mass ratio block copolymer and hydrocarbon resin is (2: 98)-(15:85). Viscosity of hydrocarbon resin is 0.1-10 p s at 160 C. Block copolymer presents as powder in composition being prepared by dry mixing. Blocks B may be hydrated by 99.5 % as calculated for origin unsaturation of ethylene bonds. Thus prepared melt composition is applied on pavement. EFFECT: improved efficiency of the method, improved quality of desired product. 17 cl, 3 tbl
机译:领域:标记路面。物质:标记铺装是通过熔化热塑性组合物来进行的。所述组合物包含具有通式(A-B)n -Sub或-(A-B)n + 1或Sub X的嵌段共聚物,其中A优选为聚(共轭乙烯基芳族)嵌段。 B优选为聚(共轭二烯)嵌段; X是多价交联剂的残基; n为1〜3的整数。嵌段A为所述嵌段共聚物的重量的8〜50质量%,嵌段共聚物的总分子量为20000〜50000,嵌段共聚物与烃树脂的质量比为(2∶98)-(15)。 :85)。烃树脂的粘度在160℃为0.1-10 p s。嵌段共聚物以粉末形式存在于通过干混制备的组合物中。嵌段B可被水合99.5%,如对于乙烯键的起始不饱和度所计算的。将由此制备的熔体组合物施加在路面上。效果:提高了方法的效率,提高了所需产品的质量。 17厘升,3汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号