METHOD AND DEVICE FOR WIRE DRAWING OF EXTRA FINE METAL WIRE

机译:超细金属线拉丝的方法和装置

摘要

PROBLEM TO BE SOLVED: To enable wire drawing for a good quality extra fine metal wire by setting an average value of a designed reduction of a wire inlet side smaller than the average value of a designed reduction of a finish wire side when a total designed reduction of a wire drawing device is divided into a wire inlet side and a wire finish side. ;SOLUTION: A wet type slip continuous wire drawing device main body 5 is arranged with dies D of ≥10 pieces. A wire rod to be drawn passes a die D1 to be coiled to a coiling block C1-1, further passing a die D2 to be coiled C2-1. The wire W successively passes a die group D to be reduced for a finished wire Wf and then is coiled. Because a speed at a wire inlet side is slow, influence resulting from slip is reduced, in the case of a small designed reduction, a wire drawing reduction is not reduced in proportion thereto, wire drawing is done without reducing a total reduction, an increase of die wear and power consumption is suppressed.;COPYRIGHT: (C)1998,JPO
机译:要解决的问题:通过将总进线率设计为比进线侧的设计减小率的平均值小,将进线侧的设计减小率的平均值设定为比精加工线的设计减小率的平均值小,以实现高质量的超细金属线的拉丝拉丝装置的线头分为导线入口侧和导线表面侧。 ;解决方案:湿式滑动连续拉丝装置主体5的D模≥10个。待拉伸的线材通过模具D 1 并卷绕到卷取块C 1 -1,进一步通过模具D 2 盘绕成C 2 -1。线材W连续地通过模具组D以减小为成品线材Wf,然后被盘绕。因为拉丝入口侧的速度慢,所以减小了由打滑引起的影响,因此在减小的设计减小的情况下,拉丝减小的比例并未与其成比例地减小,拉丝的完成并未减小总的减小,而是增加了模具磨损和功耗的抑制。.版权所有:(C)1998,日本特许厅

著录项

  • 公开/公告号JPH10192953A

    专利类型

  • 公开/公告日1998-07-28

    原文格式PDF

  • 申请/专利权人 BRIDGESTONE METALPHA KK;

    申请/专利号JP19970003706

  • 发明设计人 UEDA SHOGO;

    申请日1997-01-13

  • 分类号B21C1/00;B21C1/04;B21C1/14;

  • 国家 JP

  • 入库时间 2022-08-22 03:06:20