首页> 外国专利> RECOVERY OF WASTE RESIN BAMPER, WOODEN SYNTHETIC POWDER COMPOSED OF RECOVERED RESIN MATERIAL RECOVERED FROM WASTE RESIN BAMPER, ITS PRODUCTION AND HOLLOW WOODEN SYNTHETIC PANEL USING WOODEN SYNTHETIC POWDER

RECOVERY OF WASTE RESIN BAMPER, WOODEN SYNTHETIC POWDER COMPOSED OF RECOVERED RESIN MATERIAL RECOVERED FROM WASTE RESIN BAMPER, ITS PRODUCTION AND HOLLOW WOODEN SYNTHETIC PANEL USING WOODEN SYNTHETIC POWDER

机译:废树脂浸渍剂的回收,由废树脂浸渍剂回收的树脂材料组成的木质合成粉,其生产和使用木质合成粉的空心木质合成板

摘要

PROBLEM TO BE SOLVED: To recover a resin material to be used as a raw material by a simple and easy means by crushing a waste resin bamper into a large number of small pieces to be treated and applying compression impact force based on micro-vibration to the small pieces and further again performing crushing to crush re-crushed pieces. SOLUTION: A waste resin bamper made of polypropylene is crushed into small pieces 12 to be treated and these small pieces 12 are crushed and stretched by a compression impact force applying apparatus 30 in a primary treatment process to be formed into a thin and flat shape. The impact force applying apparatus 30 applies impact force to these small pieces 12 to be treated continuously in a rotary direction with respect to an outside compression impact member 43 and an inside compression impact member 33 having an impact surface 33a set to an outward truncated cone shape to stretch the small pieces. In a secondary treatment process, flat small pieces obtained in the primary treatment process are re-crushed and re-stretched by a compression impact force applying apparatus to be formed into a thin and flat shape (about 66mm). A recovered resin material having this thin and flat shape is crushed by a crushing means such as a cutter mill.
机译:解决的问题:通过将废树脂缓冲料粉碎成大量待处理的小块,并基于微振动施加压缩冲击力,通过简单容易的方法回收用作原料的树脂材料。将小块粉碎,然后再次进行粉碎以粉碎再粉碎的碎片。解决方案:将由聚丙烯制成的废树脂缓冲液压碎成小块12进行处理,并在初级处理过程中通过压缩冲击力施加设备30将这些小块12压碎并拉伸,以形成薄而扁平的形状。冲击力施加装置30相对于外侧压缩冲击部件43和内侧压缩冲击部件33,将这些小片12沿旋转方向连续地施加冲击力,所述外侧压缩冲击部件43和内侧压缩冲击部件33的冲击面33a为圆锥台形状。拉伸小块。在二次处理过程中,在一次处理过程中获得的扁平小片被压缩冲击力施加设备再次破碎和拉伸,从而形成薄而扁平的形状(约66mm)。具有这种薄而平坦的形状的回收树脂材料通过诸如切割机的破碎装置被破碎。

著录项

  • 公开/公告号JPH10166364A

    专利类型

  • 公开/公告日1998-06-23

    原文格式PDF

  • 申请/专利权人 AIN KOSAN KK;

    申请/专利号JP19960331895

  • 发明设计人 NISHIBORI SADAO;

    申请日1996-12-12

  • 分类号B29B17/00;B09B5/00;B29B7/92;B29B11/16;B29B13/10;B29C47/00;

  • 国家 JP

  • 入库时间 2022-08-22 03:06:19

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号