首页> 外国专利> Lightweight aggregate using fly ash and / or stone dust sludge and method for producing the same

Lightweight aggregate using fly ash and / or stone dust sludge and method for producing the same

机译:使用粉煤灰和/或石屑污泥的轻质骨料及其生产方法

摘要

The present invention relates to a lightweight aggregate using fly ash and / or a stone sludge and a method for producing the same.;The lightweight aggregate according to the present invention can be produced by adding water to fly ash, stone dust, or a mixture thereof, kneading it with a slurry, molding it into a predetermined size, drying it, and firing it at a temperature of 1100 to 1330C in air or in a reducing atmosphere do. It is also possible to add at least one kind of calcite, dolomite, montmorillonite and hematite as a foaming agent in an amount of 3 to 10 parts by weight to 100 parts by weight of fly ash, stone sludge or a mixture thereof.;According to the present invention, it is possible to provide a lightweight aggregate having excellent properties at a low cost, and at the same time, it is possible to obtain resource saving effect and waste treatment effect by recycling waste.
机译:本发明涉及一种使用粉煤灰和/或石渣的轻质骨料及其生产方法。本发明的轻质骨料可以通过向粉煤灰,石粉或混合物中加入水来生产。将其与浆液捏合,成型为预定尺寸,干燥,然后在空气或还原性气氛中于1100至1330℃下烧制。相对于100重量份的粉煤灰,石渣或其混合物,还可以以3至10重量份的量添加至少一种方解石,白云石,蒙脱土和赤铁矿作为发泡剂。对于本发明,可以以低成本提供具有优异性能的轻质集料,同时,可以通过回收废物获得资源节省效果和废物处理效果。

著录项

  • 公开/公告号KR19980033800A

    专利类型

  • 公开/公告日1998-08-05

    原文格式PDF

  • 申请/专利权人 이현구;

    申请/专利号KR19960051575

  • 发明设计人 이현구;정현희;전영석;

    申请日1996-11-01

  • 分类号C04B18/10;

  • 国家 KR

  • 入库时间 2022-08-22 02:48:20

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号