PROBLEM TO BE SOLVED: To attain dehydration solidification of high-water content soil to high-strength solidification product that is useful as a reclaiming material in situ with high volume reduction rate by adding a dehydration type solidification material to high water content soil to separate into a supernatant water phase and a mud phase and solidifying the mud phase. ;SOLUTION: (A) Soil of high water content is mixed with (B) a dehydration type solidification material [for example, comprising cement (B1), blast furnace slag (B2), and plaster (B3), when necessary, in addition, a dehydration aid such as slaked lime or aluminum polychloride (B4), and a water-reducing agent (B5) at a B1, B2, B3 weight ratio of (30-60):(25-60):(5-30), and when necessary, in addition, the components B4 and B5 are added in amounts of 1-20 wt.% and 0.1-10 wt.% based on the total of the components B1, B2 and B3, respectively. Thus, the soil of high water content separates into supernatant and mud slurry in no need of civil engineering or mechanical dehydration treatment, then the mud slurry is directly solidified in situ.;COPYRIGHT: (C)1999,JPO
机译:解决的问题:通过将脱水型固化材料添加到高含水量土壤中以分离成高水分含量的土壤,使其脱水固化成高强度固化产品,该产品可以高体积减少率就地用作再生材料。上清水相和泥浆相并固化泥浆相。 ;解决方案:(A)将高含水量的土壤与(B)脱水型固化材料[例如,必要时还包括水泥(B1),高炉矿渣(B2)和灰泥(B3)混合] ,脱水助剂如熟石灰或多氯化铝(B4)和减水剂(B5)的B1,B2,B3重量比为(30-60):( 25-60):( 5-30) ),并且在必要时,基于组分B1,B2和B3的总量,分别以1-20 wt。%和0.1-10 wt。%的量添加组分B4和B5。因此,不需要土木工程或机械脱水处理,高含水量的土壤就可以分离为上清液和泥浆,然后将泥浆直接就地固化。;版权所有:(C)1999,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号