PROBLEM TO BE SOLVED: To obtain a mixture giving a paved body improved in flow resistance, particularly flow resistance and crack resistance at a high temp., particularly crack resistance at a low temp. and prolonged in service life by forming so as to incorporate a powdery reforming material obtained by adding and dusting a specific quantity of an inorganic filler into a thermoplastic elastomer in an asphalt composition. ;SOLUTION: This asphalt mastic based mixture is formed so as to incorporate preferably 1-15 wt.%, further preferably 5-10 wt.% powdery reforming agent, which has preferably η2 mm particle diameter and is obtained by adding and dusting ≥5 pts.wt., preferably 5-30 pts.wt. inorganic filler such as a stone powder of a pulverized lime stone or other rock, slaked lime, cement, flyash, to 100 pts.wt. one or more thermoplastic elastomers of a styrene.butadiene rubber, a styrene.butadiene block, a styrene.isoprene block, an ethylene.vinyl acetate, an ethylene.ethylacrylate.;COPYRIGHT: (C)1998,JPO
机译:要解决的问题:为了获得一种铺砌体,该铺砌体的流动阻力,尤其是高温下的流动阻力和抗裂性,特别是低温下的抗裂性得到改善。并通过形成一种粉末重整材料而延长了使用寿命,该粉末重整材料是通过将一定量的无机填料添加和撒粉到沥青组合物中的热塑性弹性体中而获得的。 ;解决方案:形成该沥青胶泥基混合物,以便掺入优选1-15 wt。%,进一步优选5-10 wt。%的粉状重整剂,该粉状重整剂的粒径优选为η2mm,并且是通过添加和撒粉≥5获得的pts.wt.,优选5-30 pts.wt.。无机填料,例如粉石灰石或其他岩石的石粉,熟石灰,水泥,粉煤灰,至100pts.wt。苯乙烯-丁二烯橡胶,苯乙烯-丁二烯嵌段,苯乙烯。异戊二烯嵌段,乙烯。乙酸乙烯酯,乙烯。丙烯酸乙酯的一种或多种热塑性弹性体;版权所有:(C)1998,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号