Procedure for the treatment of Sulphide Minerals containing Gold and / or silver and at least as metal, Iron

机译:含有金和/或银以及至少作为金属,铁的硫化物矿物的处理程序

摘要

CARACTERIZADO PORQUE COMPRENDE: 1) CALCINAR EL MINERAL GRANULADO QUE CONTIENE ORO Y/O PLATA Y POR LO MENOS HIERRO COMO METAL ACOMPANANTE A TEMPERATURAS ENTRE 500�C Y 900�C ANADIENDO GAS QUE CONTIENE OXIGENO EN UN LECHO FLUIDIZADO CIRCULANTE PARA FORMAR UNA MEZCLA DE MATERIA SOLIDA (MMS) CON CONTENIDO DE OXIDOS METALICOS Y UN GAS DE ESCAPE QUE CONTIENE SO2; 2) ENFRIAR LA (MMS) PROCEDENTE DE LA CALCINACION EN POR LO MENOS 50�C; 3) CARGAR LA (MMS) ENFRIADA A UN REACTOR DE LECHO FLUIDIZADO E INTRODUCIR EN DICHO REACTOR GAS DE ESCAPE QUE CONTIENE SO2 Y EL SO3 FORMADO POR OXIDACION CATALITICA FUERA DEL REACTOR DE LECHO FLUIDIZADO DE PARTE DEL SO2 PRESENTE EN EL GAS DE ESCAPE, PARA TRANSFORMAR A TEMPERATURAS ENTRE 250�C Y 650�C LOS OXIDOS METALICOS PRESENTES EN LA (MMS) EN SULFATOS METALICOS Y LIGAR EN FORMA DE SULFATO METALICO POR LO MENOS EL 10% DEL CONTENIDO DE AZUFRE DEL GAS DE ESCAPE; 4) EXTRAER DEL REACTOR LA (MMS) CON CONTENIDO DE SULFATO METALICO Y AGITARLA CON UNA SOLUCION ACIDA ACUOSA PARA DISOLVER EN ELLA EL SULFATO METALICO; Y 5) RETIRAR LAS MATERIAS SOLIDAS DE LA SOLUCION PARA SER ALIMENTADAS A UNA INSTALACION DE EXTRACCION DE ORO Y/O PLATA, EN ESPECIAL LIXIVIACION CON CIANURO
机译:其特征包括:1)在500°C和900°C的温度范围内,计算出粉状含矿物质中的含矿物质的金和/或银,以及至少铁作为伴生金属。具有金属氧化物和含SO2的废气的固体(MMS); 2)冷却至少50°C时产生的(MMS); 3)将(MMS)冷却液充入流化床反应器中,并从流态化床反应器中引入一部分由SO2和SO3催化的氧化气体,其中SO2和SO3的催化氧化作用来自流化床反应器中的SO2和SO3在250°C和650°C的温度下将(MMS)中存在的金属氧化物转变为金属硫酸盐,并以金属硫酸盐的形式结合,至少占排气中硫含量的10%; 4)用反应器中的金属硫酸盐去除(MMS),并用酸水溶液摇匀,以溶解金属硫酸盐;和5)从溶液中去除固体物质,以提供给金和/或银提取设施,特别是与氰化物一起浸出

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号