A heat-resistant alloy suitable as a material for reactor tubes such as cracking tubes for producing ethylene in the petrochemical industry comprises, in % by weight, 0.1 to 0.5% of C, over 0% to not more than 4% of Si, over 0% to not more than 3% of Mn, over 40% to not more than 50% of Cr, over 0% to not more than 10% of Fe, 0.01 to 0.6% of Ti, 0.01 to 0.2% of Zr, at least one element selected from the group consisting of 0.5 to 5% of W, 0.3 to 2% of Nb and 0.5 to 3% of Mo, and the balance substantially Ni. The alloy is excellent in oxidation resistance, high-temperature creep rupture strength, carburization resistance and ductility after aging.