The present invention relates to a loess composition for preventing shrinkage cracking due to moisture evaporation and a method for the construction of a loess soil, comprising 97.6 to 99.99 parts by weight of loess; 2.4 to 0.01 parts by weight of a mixture A consisting of hydrated alkaline silicate, 1 to 3% by weight of kaolin, 4 to 6% by weight of diazonaphthalene, 12 to 16% by weight of sulfonic acid and 75 to 83% by weight of water; And the loess composition containing 10 to 1000 times water based on the weight of the mixture A and the loess composition are applied to the floor and then subjected to compaction after 15 to 50 hours have elapsed.;In the case of using the loess composition, it is possible to prevent the leakage of water and gas by suppressing shrinkage cracks generated during drying, and to improve appearance.
机译:本发明涉及一种用于防止由于水分蒸发而引起的收缩裂缝的黄土组合物和一种用于建造黄土土壤的方法,其包含97.6至99.99重量份的黄土。 2.4至0.01重量份的混合物A,其由水合的碱性硅酸盐,1至3重量%的高岭土,4至6重量%的重氮萘,12至16重量%的磺酸和75至83重量%的混合物组成水然后,将基于混合物A和黄土组合物的重量将含有10至1000倍水的黄土组合物施用于地板上,然后在经过15至50小时后进行压实;在使用黄土组合物的情况下,通过抑制干燥时产生的收缩裂纹,可以防止水和气体的泄漏,并且可以改善外观。

著录项

  • 公开/公告号KR19980084228A

    专利类型

  • 公开/公告日1998-12-05

    原文格式PDF

  • 申请/专利权人 임병국;

    申请/专利号KR19970019944

  • 发明设计人 임병국;

    申请日1997-05-22

  • 分类号C04B14/10;

  • 国家 KR

  • 入库时间 2022-08-22 02:18:50

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号