首页> 外国专利> Surface hardening method of cobalt-chromium-tungsten main alloy

Surface hardening method of cobalt-chromium-tungsten main alloy

机译:钴铬钨主合金的表面硬化方法

摘要

The present invention relates to a method of hardening the surface of a cobalt-chromium-tungsten-based main alloy, and its object is to form a surface hardened layer by using a plasma of a DC pulse control method, so that there is no distortion of the material, and environmental problems It is an object of the present invention to provide a surface hardening method of a Co-Cr-W based main alloy in which a surface hardening layer having a uniform thickness can be obtained even in a complicated shape.;The present invention for achieving the above object in the method for curing the surface of the Co-Cr-W-based main alloy, using a pulse-controlled direct current, the treatment temperature is set to 550 ~ 700 ℃, the treatment gas 100% N 2 gas and the H 2 or by a gas containing N 2 gas of 75% or less of the surface hardening method of the Co-Cr-W-based cast alloy, characterized in that to perform a plasma nitriding treatment in the invention.
机译:本发明涉及一种使钴-铬-钨基主合金的表面硬化的方法,其目的是通过使用DC脉冲控制方法的等离子体来形成表面硬化层,从而不产生变形。本发明的目的是提供一种Co-Cr-W基主合金的表面硬化方法,其中即使在复杂的形状中也可以获得具有均匀厚度的表面硬化层。 ;为了达到上述目的的本发明,在Co-Cr-W基主体合金的表面固化方法中,使用脉冲控制的直流电,将处理温度设定为550〜700℃,将处理气体100%N 2 气体和H 2 气体或含有N 2 气体且其表面硬化方法的75%以下的气体Co-Cr-W基铸造合金,其特征在于在本发明中进行等离子体氮化处理。

著录项

  • 公开/公告号KR19990052217A

    专利类型

  • 公开/公告日1999-07-05

    原文格式PDF

  • 申请/专利权人 이구택;신현준;

    申请/专利号KR19970071672

  • 发明设计人 김영섭;박정렬;

    申请日1997-12-22

  • 分类号C21D1/06;C22F1/10;C22F1/11;

  • 国家 KR

  • 入库时间 2022-08-22 02:17:00

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号