首页> 外国专利> AL-CU-LI ALLOYS WITH IMPROVED CRYOGENIC FRACTURE TOUGHNESS

AL-CU-LI ALLOYS WITH IMPROVED CRYOGENIC FRACTURE TOUGHNESS

机译:具有改善的低温断裂韧性的AL-CU-LI合金

摘要

FIELD: nonferrous metallurgy. SUBSTANCE: aluminum-based alloy containing 2.0 to 6.5 weight parts of copper and 0.2 to 2.7 weight parts of lithium is prepared by heating solid solution, hardening it in water, and at least once deforming and artificially aging it to an extent sufficient to provide strength and fracture toughness at cryogenic temperature equal to or exceeding the same characteristics at room temperature. In addition, invention is distinguished by composition of alloy being deformed and by container to store cryogenic material. EFFECT: increased strength and fracture toughness at cryogenic temperatures. 35 cl, 7 dwg, 3 tbl, 26 ex
机译:领域:有色冶金。物质:通过加热固溶体,使其在水中硬化,至少变形一次并人工老化至足以提供强度的程度,来制备包含2.0至6.5重量份的铜和0.2至2.7重量份的锂的铝基合金。低温下的断裂韧性等于或超过室温下的相同特性。另外,本发明的特征在于变形的合金成分和用于储存低温材料的容器。效果:在低温下增加强度和断裂韧性。 35厘升,7公升,3汤匙,26厘

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号