首页> 外国专利> continuous casting method of the thin-walled steel hollow ingot

continuous casting method of the thin-walled steel hollow ingot

机译:薄壁空心钢锭的连续铸造方法

摘要

continuous casting method of the thin-walled steel hollow bars mainly with ratio of diameter to thickness of the wall, equal to 15 to 40, which includes heating u0437u0430u0442u0440 awka, u0437u0430u043bu0438u0432u043au0443 liquid metal u043au0440u0438u0441u0442u0430u043bu043bu0438u0437u0430u0442u043eu0440 dorn and the lengthening bars with the fact that, in order to ensure the stability of process heat appetizer to u0442u0435u043cu043fu0435u0440u0430u0442u0443u0440u044bt = 530 + 8D / b - 2,5t, where t is the temperature of heating free,hail; d is the diameter of the bars, mm; b - wall thickness hollow ingot, mm, t is the temperature of heating the liquid metal, the hail.
机译:薄壁空心钢的连续铸造方法,主要是直径与壁厚之比等于15到40,包括加热 u0437 u0430 u0442 u0440 awka, u0437 u0430 u043b u0438 u0432 u043a u0443液态金属 u043a u0440 u0438 u0441 u0442 u0430 u043b u043b u0438 u0437 u0430 u0442 u043e u0440磨损并加长杆,以确保过程热开胃器对 u0442 u0435 u043c u043f u0435 u0440 u0430 u0442 u0443 u0440 u044bt = 530 + 8D / b-2,5t的稳定性,其中t是自由加热的温度, ; d是钢筋的直径,mm; b-空心锭的壁厚,mm,t是加热液态金属的冰雹温度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号